dc.contributor.authorCender, E. Uslu-
dc.contributor.authorGuler, C.-
dc.contributor.authorOdabasi, D.-
dc.date.accessioned2023-01-06T08:48:16Z-
dc.date.available2023-01-06T08:48:16Z-
dc.date.issued2021-
dc.identifier.citationCender, EU., Guler, C., Odabasi, D. (2021). The Effects of Polymerization Mode and Layer Thickness on Monomer Released from Bulk Fill Composite Resins. Nigerian Journal of Clinical Practice, 24(10), 1442-1449. Doi:10.4103/njcp.njcp_676_20en_US
dc.identifier.isbn1119-3077-
dc.identifier.urihttp://dx.doi.org/10.4103/njcp.njcp_676_20-
dc.identifier.urihttps://www.webofscience.com/wos/woscc/full-record/WOS:000751363200005-
dc.identifier.urihttps://pubmed.ncbi.nlm.nih.gov/34657008-
dc.identifier.urihttp://earsiv.odu.edu.tr:8080/xmlui/handle/11489/3334-
dc.descriptionWoS Categories : Medicine, General & Internal Web of Science Index : Science Citation Index Expanded (SCI-EXPANDED) Research Areas : General & Internal Medicineen_US
dc.description.abstractBackground: Residual monomers released from composite resins have cytotoxic, mutagenic, and estrogenic effects. Mode of polymerization and application thickness are important for monomer release. Aims: The aim of this study was to investigate the effects of different modes of a third-generation light-curing unit (LCU) and layer thickness on residual monomer released from two different bulk-fill composite resins. A total of 80 samples were prepared for each bulk-fill composite using a mold. Each bulk-fill composite was divided into four groups according to polymerization mode (standard and extra power) and layer thickness (2 and 4 mm). In addition, four groups were divided into four subgroups according to time periods (1 h, 24 h, 3 days, and 7 days). Methods and Material: The samples were polymerized with VALO LED device. The amount of residual monomer was measured with High-Performance Liquid Chromatography (HPLC). All statistical analyses were processed using SPSS Version 23.0. The normal distribution of data was confirmed using Kolmogorov-Smirnov Normal Distribution Test and Shapiro-Wilk Normal Distribution Test. When the distribution was normal, parametric tests, Student's t test and one-way ANOVA, were used. When the distribution was not normal, non-parametric tests, Mann-Whitney U test, and Kruskal-Wallis testwere used. Results: It was found that the standard mode of LCU produced lower amounts of TEGDMA, Bis-GMA, and UDMA in both composite materials. In addition, when the layer thickness increased, TEGDMA, Bis-GMA, and UDMA releases increased, too. Conclusions: This study revealed that the amount of residual monomers released from bulk-fill composites was affected by layer thickness and polymerization time.en_US
dc.description.sponsorshipFunding Orgs : Ordu University, Scientific Research Coordination Unit [A1817] Funding Name Preferred : Ordu University, Scientific Research Coordination Unit(Ordu University) Funding Text : Ordu University, Scientific Research Coordination Unit (Project No: A1817).en_US
dc.language.isoengen_US
dc.publisherWOLTERS KLUWER MEDKNOW PUBLICATIONS MUMBAIen_US
dc.relation.isversionof10.4103/njcp.njcp_676_20en_US
dc.rightsinfo:eu-repo/semantics/openAccessen_US
dc.subjectHPLC ANALYSIS; ELUTION; HALOGEN; BISGMA; TEGDMAen_US
dc.subjectBulk-fill composite; HPLC; layer thickness; polymerization mode; residual monomeren_US
dc.titleThe Effects of Polymerization Mode and Layer Thickness on Monomer Released from Bulk Fill Composite Resinsen_US
dc.typearticleen_US
dc.relation.journalNIGERIAN JOURNAL OF CLINICAL PRACTICEen_US
dc.contributor.departmentOrdu Üniversitesien_US
dc.identifier.volume24en_US
dc.identifier.issue10en_US
dc.identifier.startpage1442en_US
dc.identifier.endpage1449en_US
Appears in Collections:Diş Hastalıkları veTedavisi

Files in This Item:
There are no files associated with this item.


Items in DSpace are protected by copyright, with all rights reserved, unless otherwise indicated.